Delivering High Quality Stainless Steel and Alloy Piping Products — Pipes, Tubes, Fittings, Flanges and more for Global Industries.
sales@savoypipinginc.com
Savoy Piping Inc. supplies ASTM A213 T9 / ASME SA213 Grade T9 seamless chrome moly tubes — the 9Cr-1Mo grade specified when heater and high-temperature exchanger tubes need stronger sulfidation and oxidation resistance than 5Cr material.
T9 is a deliberate chemistry choice for severe elevated-temperature process duty. Procurement usually focuses on OD/wall, heat treatment, hardness, and clean mill chemistry — not generic “alloy tube” wording. For IBR-linked boiler packages, confirm SA213 T9 documentation requirements early.
Where T9 fits: severe refinery heater tubes, high-temperature process exchangers, and furnace tubing exposed to sulfur-bearing streams. Milder duties may stay on T5. Power-plant steam tubing more often uses T11, T22 or CSEF T91.
Matching pipe grade is typically ASTM A335 P9. We supply T9 with EN 10204 3.1 / 3.2 certificates and optional third-party inspection.
Also see: Alloy steel seamless hub · Chrome moly hub · Materials hub.
| A213 T9 Alloy Steel Seamless Tubes Specification | ASTM A213 / ASME SA213 |
| A213 T9 Alloy Steel Seamless Tubes Grades | ASTM A213 T5, ASTM A213 T9, ASTM A213 T11, ASTM A213 T22, ASTM A213 T91, ASME SA213 T5, ASME SA213 T9, ASME SA213 T11, ASME SA213 T22, ASME SA213 T91 |
| A213 T9 Alloy Steel Seamless Tubes Type | Seamless - Hot Rolled / Cold Drawn |
| A213 T9 Alloy Steel Seamless Tubes Outer Diameter Size | A213 - 3/8" NB to 30" NB (Nominal Bore Size) |
| A213 T9 Alloy Steel Seamless Tubes Wall Thickness | Schedule 20 to Schedule XXS (Heavier On Request) Up to 250 mm Thickness |
| A213 T9 Alloy Steel Seamless Tubes Length | 5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size. |
| A213 T9 Alloy Steel Seamless Tubes Pipe Ends | Plain Ends / Beveled Ends / Coupling |
| A213 T9 Alloy Steel Seamless Tubes Delivery Conditions | As Rolled, Cold Drawn, Normalizing Rolled, Thermomechanical Rolled / Formed, Normalizing Formed, Normalized and Tempered / Quenched and Tempered - BR / N / Q /T |
| A213 T9 Alloy Steel Seamless Tubes Coating | Epoxy Coating / Colour Paint Coating / 3LPE Coating. |
| A213 T9 Alloy Steel Seamless Tubes Other Testing | Tensile Test, Transverse Tension Tests, Flattening Test, Metal Structure and Etching Tests, Photomicrographs, Hardness Tests, etc. |
| A213 T9 Alloy Steel Seamless Tubes Dimension | All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM, ASME, API. |
| A213 T9 Alloy Steel Seamless Tubes Value Added Services | Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Galavanizing / Heat Treatment |
| A213 T9 Alloy Steel Seamless Tubes Packaging | Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector |
| A213 T9 Alloy Steel Seamless Tubes Shipment & Transportation | By Road - Truck / Train, By Sea - Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 4 Feet Container / High Cube Container / Open Top Container, By Air - Freighter Civil Passenger and Cargo Planes |
| A213 T9 Alloy Steel Seamless Tubes Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS ETC |
ASTM A213 / ASME SA213 Grade T9 is seamless ferritic alloy-steel tubing for boilers, superheaters and heat exchangers, commonly described as 9Cr-1Mo. Higher chromium versus T5 improves resistance to high-temperature oxidation and sulfidation; molybdenum supports strength at temperature.
T9 is related to pipe grade A335 P9, but ordered as tube product for heat-transfer equipment. Do not confuse classic T9 with CSEF grade T91 — both are roughly 9% Cr, yet chemistry, heat treatment and creep design intent differ.
Use T9 when process corrosion drives 9Cr-1Mo tube selection. Use T5 for many standard heater duties. Use T91 when creep-strength-enhanced modified 9Cr is required for supercritical steam tubes — not as a casual substitute for classic T9 heater tubing.
| Composition, % | |||||||||||||
| Grade | UNS Designation | Carbon | Manganese | Phosporus | Sulphur | Silicon | Nickel | Chromium | Molybdenum | Vanadium | Niobium | Aluminium | Other Elements |
| T5 | K4154 | 0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50 | … | 4.00-6.00 | 0.4-0.65 | … | |||
| T9 | K90941 | 0.15 max | 0.30-0.60 | 0.025 | 0.025 | 0.25-1.00 | … | 8.00-10.00 | 0.90-1.10 | … | |||
| T11 | K11597 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50-1.00 | … | 1.00-1.50 | 0.44-0.65 | … | |||
| T22 | K2159 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50 | … | 1.9-2.60 | 0.87-1.13 | … | |||
| T91 | K991 | 0.07-0.14 | 0.30-0.60 | 0.02 | 0.010 | 0.20-0.50 | 0.4 | 8.0-9.5 | 0.85-1.05 | 0.18-0.25 | 0.06-0.10 | 0.02 | Ti 0.01 ZR 0.01 |
| Hot rolled | Outside Diameter, mm | Tolerance, % |
| OD≤101.6, WT≤2.4 | +40/-0 | |
| OD≤101.6, 2.4<WT≤3.8 | +35/-0 | |
| OD≤101.6, 3.8<WT≤4.6 | +33/-0 | |
| OD≤101.6, WT>4.6 | +28/-0 | |
| OD>101.6, 2.4<WT≤3.8 | +35/-0 | |
| OD>101.6, 3.8<WT≤4.6 | +33/-0 | |
| OD>101.6, WT>4.6 | +28/-0 | |
| Cold Drawn | Outside Diameter, mm | Tolerance, % |
| OD≤38.1 | +20/-0 | |
| OD>38.1 | +22/-0 |
| Hot rolled | Outside Diameter, mm | Tolerance, mm |
| OD≤101.6 | +0.4/-0.8 | |
| 101.6<OD≤19.5 | +0.4/-1.2 | |
| 19.5<OD≤228.6 | +0.4/-1.6 | |
| Cold Drawn | Outside Diameter, mm | Tolerance, mm |
| OD<25.4 | ±0.10 | |
| 25.4≤OD≤38.1 | ±0.15 | |
| 38.1<OD<50.8 | ±0.20 | |
| 50.8≤OD<63.5 | ±0.25 | |
| 63.5≤OD<76.2 | ±0.30 | |
| 76.2≤OD≤101.6 | ±0.38 | |
| 101.6<OD≤19.5 | +0.38/-0.64 | |
| 19.5<OD≤228.6 | +0.38/-1.14 |
S1. STRESS-RELIVED ANNEALED Tubes
S2. STABILIZING HEAT TREATMENT
S3. UNSTRAIGHTENED Tubes
S4. INTERNGRANULAR CORROSION TEST
ASTM A213 T9 (9Cr-1Mo) seamless tubes are used in high-temperature heaters, boilers and heat exchangers where higher chromium is needed for oxidation and sulfidation resistance, especially in severe refinery heater service.
T5 (5Cr-0.5Mo) covers many heater and exchanger duties. T9 (9Cr-1Mo) is selected when corrosion/sulfidation risk is higher and the design calls for more chromium. Follow the project corrosion class; do not substitute on price alone.
No. Both are roughly 9% chromium alloys, but T91 is a vanadium-niobium modified CSEF steel for high-creep steam service. Classic T9 is the traditional 9Cr-1Mo process/heater grade. Chemistry, heat treatment and welding practice differ.
Yes. We supply ASTM A213 / ASME SA213 T9 seamless tubes with mill test certificates and optional IBR / third-party inspection packages as specified on the purchase order.
We Export ASTM A213 T9 Alloy Steel Tubes to Saudi Arabia, Iran, Iraq, United Arab Emirates, Qatar, Bahrain, Oman, Kuwait, Turkey, Egypt, Yemen, Syria, Israel, Jordan, Cyprus, Singapore, Malaysia, Indonesia, Thailand, Vietnam, South Korea, Japan, Sri Lanka, Maldives, Bangladesh, Myanmar, Taiwan, Cambodia, Argentina, Bolivia, Brazil, Chile, Venezuela, Colombia, Ecuador, Guyana, Paraguay, Uruguay, United States of America, Canada, Mexico, Panama, Costa Rica, Puerto Rico, Trinidad And Tobago, Jamaica, Bahamas, Denmark, Russia, Norway, Germany, France, Italy, United Kingdom, Spain, Ukraine, Netherlands, Belgium, Greece, Czech Republic, Portugal, Hungary, Albania, Austria, Switzerland, Slovakia, Finland, Ireland, Croatia, Slovenia, Malta, Nigeria, Algeria, Angola, South Africa, Libya, Egypt, Sudan, Equatorial Guinea, The Republic Of Congo, Gabon, Europe, Africa, Asia, North America, South America, Middle East, Far East.etc
Savoy Piping Inc. is a well known worldwide Exporter of ASTM A213 T9 Alloy Steel Seamless Tubes, Savoy Piping Inc. is committed to provide each and every customer with the highest standard of customer service. We deal in A213 T9 Alloy Steel Seamless Tubes in India and Overseas, offering a wide range of ASTM A213 T9 Alloy Steel Seamless Tubes